A5.5 E11018-M, easy to order.
On Wednesday, June 12, 2019 at 12:22:55 PM UTC+7, Ehab Ahmed wrote:
-- Cooling rate control is important and PWHT to reduce stress.
On Wednesday, June 12, 2019 at 12:22:55 PM UTC+7, Ehab Ahmed wrote:
Dear Sirs,Pleas help me to Select electrode ? for AISI 4130 (70-75 Ksi) and API 5CT L80 Pipe materials to weld by SMAW.Using ASME IX Code.Thanks and Best Regards,Ehab Ahmed