Thursday, June 6, 2019

Re: [MW:29681] PWHT Chart Recorder Calibration

You will get that information PFI Standard

Temp. recording instrument is 6 month

AWS D10.10 you can check also



On Sun, Jun 2, 2019 at 9:42 PM Revdiwala Darshan <darshanmrevdiwala@gmail.com> wrote:
Dear Experts,
Can anyone suggest, which standard need to be followed for PWHT chart recorder calibration with use of Simulator.

Regards, 
Darshan

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABDq6gj-wuZ5xPg8c%2BgG_LLckLJcHFhRBR0ucHa2CBjjkzwtbw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8njVbVGn3s3f%2B_iRf22Cg1z2uzJKFb%3DrLgOda6V717ijg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...