Dear Ali,
Rep a-1) & a-2) I suggest you, go through ASME BPVC Sec. V, nonmandatory appendix B of article 4.
b) Whould you please introduce the reference? Generally the probe angle is not the most important factor affecting the mode conversion.
c) The first thing which will help the interpreter is imagination of the sound interaction with the workpiece. In addition the information about the base material and its capability to mode conversion, the probable defects, the geometrical parameters and …
Regards
On Sun, May 27, 2018 at 10:17 AM, Ali Asghari <asgharialigl@gmail.com> wrote:
Dear All.--a)Would you clear and explain these two paragraphs:1.Measurements of beam spread for scan indexing limits shall be taken only when required by a referencing code section. Beam spread angles shall be measured once for a search unit wedge combination in the calculated far field at the beginning of each period of extended use, or every 3 months, whichever is less.(what is scan indexing limits and when is it used and how can be specified and based on which standard?)2.Alternative methods of distance-amplitude of correction of sensitivity may be used provided the results are as reliable as those obtained by the acceptable method. In addition, the alternative method and its equipment shall meet all the performance requirements of this standard.(which alternative method of sensitivity calibration and in which standard are explained except as AWS D1.1)b)and why mode conversion is more important and higher probable to happen for Probe 60 degree especially for corner square speciemen?c) when the mode conversion in practical cases you have experienced mode conversion and get false indications and how find?Regards.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
M. Shokri Arfaei
ASNT NDT Level III
International Welding Engineer
Mob.:+98 912 1394023
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments