Re: [MW:27842] Re: If a welder is qualified with SS (Stainless Steel) GTAW, He can weld CS Carbon steel GTAW?
HI Srinivas,
Pl find the below table extract from ASME Sec.IX QW-20 Base Metal Grouping, if you qualified any one group P-1 to P-15F means he can weld upto P1- to P15F grouping metals
On Sat, May 12, 2018 at 11:21 AM, srinivas <SrinivasDuraisamy@gmail.com> wrote:
--Hi ,I have welder qualification P4 to P4 material. He can weld P5A materials ?. Plz give some reference though ASMEThanks,Srinivas.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments