Friday, May 18, 2018

Re: [MW:27861] Weld Managment Software

Dear Mr. Slavik,
So many softwares available in EPC companies for welding and also covering material receiving  activity to final release.
The bad thing us administration or authorized person can change data in soft form.
The good thing is each and every activity or information in summarized.  
Regards,
M.Babur Khan

Sent from my iPhone

On 18 May 2018, at 3:57 PM, Slavik Borisov <slavikborisov5@gmail.com> wrote:

Does any one on here use a specific type of weld management software. If so, which one and what do you like about it? and what don't you like about it? not looking to create WPS and PQR just looking to put all of our welding documentation in a centralized location.

Thanks,

Slavik Borisov

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...