Thursday, May 24, 2018

Re: [MW:27879] AWS D 1.1 interpretation on Increase in Preheat / Interpass temperature

Dear Prasad
Appreciate your feed back on the solution.

Dear members 

Follow up with a brief note on the solution (The Most Important) is always recommended for the benefit of others.

Send a note after the problem has been solved to all who helped you; let them know how it came out and thank them again for their help. If the problem attracted general interest, it's appropriate to post the follow-up here.


On Thursday, 24 May 2018 09:19:08 UTC+4, N V PRASAD wrote:
Dear All,

It was good debate and the explanations were awesome.  Our team from US,  has discussed with  AWS Committee member and  it was clarified that the increase is applicable for Inter pass temperature only.

Regards

Prasad


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...