MIT exempt per UCS-66 Curve 'D'

On Sat, May 26, 2018 at 11:15 PM, vishnudas balachandran <vishnudasb@gmail.com> wrote:
Dear All,
Vessel Data,
MDMT = ( - 30 Deg C),
Plate thickness = 12mm,
Dished end = 12/14,
Material = SA 516 Gr.70 N.+ HIC
Design Code - ASME Sec VIII DIV 1.

Is Impact testing required ?
As per UG-20 (f) (3) ,
"Design temperature is no warmer than 650°F (345°C) nor colder than −20°F (−29°C). Occasional operating temperatures colder than −20°F (−29°C) are acceptable when due to lower seasonal atmospheric temperature."

Is there any provision for wave Impact testing as per code provision(s). Kindly advise.

--
Regards,

Vishnu



*Before printing, think about your ENVIRONMENTAL responsibility!Don't print unless necessary.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...