The interpretation on paragraph QW-424 given by the partner
Shyam Krishnan is correct!

2018-05-24 7:11 GMT-05:00 Vanchinath S.A. <vanchinaths@gmail.com>:
Yes. You are right.

On Thu, 24 May 2018, 17:20 Shyam Krishnan, <shyamkrishnan7@gmail.com> wrote:
Dear Vanchi Sir,

My interpretation is 
, if we are welding(PQR) between P-1 to P-22, and qualify the procedure , then my PQR is qualified for any metal from P-1 to any metal from P-22 .
Is this right?

Shyam


On Thu, May 24, 2018 at 3:57 PM, Vanchinath S.A. <vanchinaths@gmail.com> wrote:
Your interpretation is not right.

On Thu, 24 May 2018, 15:41 Aakash, <harenathjha@gmail.com> wrote:

Hello All,

I was going through the ASME section IX-2017 edition QW-424, Please see the circled part,
 My interpretation is , if we are welding(PQR) between P-1 to P-22, and qualify the procedure , then my PQR is qualified for P-1 to P-1 and P-22 to P-22 also.

Please let me know that my interpretation is correct or not ?

Regards
AAkash



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--

Ing. José Juan Jiménez Alejandro

ASME Independent Consultant 

and Technical Manager SSI-TPI

Cel. +52 812 352 4606

Skype: jjjimeneza

Twitter: @jjjimeneza



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...