Re: [MW:27865] minimum distance limitation between two weld joints

Friends a warm greeting to the whole group.

I have seen different publications regarding the minimum distance between welds, in this forum regarding this debate.

Of all the comments, the one that I find most convincing is the one expressed by comrade Srirammadhan in March of 2012, which says that it must be 1.5 times the outside diameter of the pipe or 5 times the thickness of the base metal or pipe, the greater of both values.

Then the friend Veereswara Rao on April 17, 2018, asks if there is a norm of reference in this respect, in fact according to the response of the friend kannayeram gnanapandithan if there is reference to a norm that supports it (Ref BS EN 12952-5), what which I think is excellent, because it must be that way, because each criterion or rule must be backed by a rule in a certain code that is being used. In the debate that opened the friend Murat Aksoy in March 2012 I consulted for the code ASME B31.3 or EN.

Now, this same criterion quoted from the reference Ref BS EN 12952-5, can be used for ASME B31.3 ??? or can it even be used for ASME B31.8 ????

In our case we use as a criterion that the minimum distance between two welds is 1 time the outer diameter of the pipe or base metal or 12 times the thickness of the same, the greater of both values, this as best practice, but the weakness of this criterion is that it lacks support, that is, it has the weakness that it does not have or at least does not achieve an endorsement in a Standard, either in ASME Code B31.3 or B31.8.

It is for this reason that I consider Comrade Srirammadhan's comment to be strong because it has a basis and support. I also respect all the comments of the participants of this debate in the forum. But like the criterion that I stated, any criterion without endorsement of reference to norm becomes only a best practice.

I apologize if I do not know that the rest of the comments on the subject also have reference to some standard as a backup in a certain code that is being used.

Please comment and also clarify what criteria can be used for ASME B31.8.

regards
Castle

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...