Dear Experts,
Mistakenly used the below Welding consumables for Welding of ASTM A333 Gr 6 flare stack field Weld,
Filler wire for root and hot pass: ER80SB2 and fill and cap passes: E8018 B2.
Kindly provide your valuable suggestions whether this can be acceptable?
What will happen to the properties of the weld metal?
Can use the same weld? Or need to cut out.
Thanking you
P Govindan