[MW:27895] TANK BOTTOM PLATE REPAIR - REG

Dear Experts,
                       During sutdown after blasting  tank bottom plates we observed lot of pitting corrosion. Some pitting are went through the entire thickness and some pittings are in the half way of the thickness. 

By following API 653 is it possible to repair with patch plate on the holes formed and went through the entire bottom plate thickness by pitting corrosion. Your kind suggestion is requested.
Tank Construction code: API -650
Bottom plate thickness - 8mm

With Regards,
N.S




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...