[MW:27892] Re: LOW HUMIDITY - LOW DEW POINT ARGON

Please use 99.9999% ( Argan 6.0) pure argon to avoid porosity and other humidity related defects..

Regards
Pratish

On Saturday, May 19, 2018 at 6:15:23 AM UTC, hanyon wrote:
Dear All 

Do you have specification or any technical information about LOW HUMIDITY - LOW DEW POINT ARGON To be sued for MIG  Aluminum welding To eliminate porosity and inclusions 

BR
HA 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...