[MW:27828] Hydro test with Normal Water

Dear Experts,

We are installing HRSG (Heat Recovery Steam Generator) consist of Alloy Steel (P11, P22) and Carbon steel SA106 Gr.B tube bundles.

 In our past experience we did hydro test with demineralized water (DM) but in current project there is scarcity in procuring of DM water can we proceed with Hydro test with Normal RO water.

IF not water are major consequences to tube bundles.

Regards
G.Mohanraj

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...