Friday, May 18, 2018

Re: [MW:27856] If a welder is qualified with SS (Stainless Steel) GTAW, He can weld CS Carbon steel GTAW?

Provided other essential variable are met

On Fri, 18 May 2018 8:19 am guru vasanth, <guruvasanth@gmail.com> wrote:
See below table for welding variables for welders . Any change in essential variable ,is required requalification.

Thanks and regards

Guru Sundara Mahalingam



Best regards

Guru S Mahalingam

On Sat, Feb 24, 2018 at 11:11 AM, PK M <pkmqaqc@gmail.com> wrote:
Dear Sir,

If a welder is qualified with SS (Stainless Steel) GTAW,  He can weld CS Carbon steel GTAW? Need code Referance...

Thanks.
PKM

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...