Dear Experts,
we should note that it also depends impact requirements and the respective group number.
if impact property is required, the applicable group number become part of the requirement.
if you qualify p-1 group-1 and the impact property is required, you cannot use the same procedure to weld p-1 group-2.

On ‎Thursday‎, ‎24‎ ‎May‎ ‎2018‎ ‎13‎:‎18‎:‎02‎ ‎WAT, Vanchinath S.A. <vanchinaths@gmail.com> wrote:


Yes. You are right.

On Thu, 24 May 2018, 17:20 Shyam Krishnan, <shyamkrishnan7@gmail.com> wrote:
Dear Vanchi Sir,

My interpretation is 
, if we are welding(PQR) between P-1 to P-22, and qualify the procedure , then my PQR is qualified for any metal from P-1 to any metal from P-22 .
Is this right?

Shyam


On Thu, May 24, 2018 at 3:57 PM, Vanchinath S.A. <vanchinaths@gmail.com> wrote:
Your interpretation is not right.

On Thu, 24 May 2018, 15:41 Aakash, <harenathjha@gmail.com> wrote:

Hello All,

I was going through the ASME section IX-2017 edition QW-424, Please see the circled part,
 My interpretation is , if we are welding(PQR) between P-1 to P-22, and qualify the procedure , then my PQR is qualified for P-1 to P-1 and P-22 to P-22 also.

Please let me know that my interpretation is correct or not ?

Regards
AAkash



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...