Tuesday, February 27, 2018

Re: Re: [MW:27397] change in electrode class


7018- F4 
6013 -F2 

F4 with backing qualifies F2 with backing
F4 without backing qualifies F2 With backing

On Mon, Feb 26, 2018 at 9:37 PM, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Check F no

On 26-Feb-2018 7:06 pm, "praveen nair" <pk13890@gmail.com> wrote:

Dear Sir,

 Welder is Qualified in E 7018 can also be qualify in E 6013 

 


Praveen Nair
 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
selastine sudhakar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...