Diff btwn "Torquing & Tensioning :

Basically definitions :

Torquing is "The loading / stressing bolts using using manual or hydraulic torque wrenches".

Tensioning is loading / stressing bolts using hydraulic jacking tools. 

Tightening can be defined as "The making tight of flange joint by torquing or tensioning the bolts"

Bolts shd b tightened in a controlled sequence as under : 

E.g. 4 bolts flange : 1 -3 -2- 4
16 bolt flange: 1- 9 -5- 13- 3 -11 -7- 15 -2 -10- 6- 14- 4 -12 -8- 16
32 bolts flange : 1 -17 -9 -25 -5 -21 13 29 3 19 11 27 7 23 15 31 2 18 10 26 6 22 14 30 8 24 16 32 4 20 12 28

Regards 

Chandrakant Mohikar
Ex. CSR-. (PDO / VELOSI ) & BP / QP, TOOTAL, Bechtel

+91 8446079514

On 25 Feb 2018 7:02 p.m., "Thompson, Dennis" <Dennis.Thompson@teaminc.com> wrote:

PK M,

 

Bolt torqueing refers to the circumferential moment (ft-lbs, or m-N) exerted on a bolt-nut assembly, or on a bolt and threaded-hole assembly, to tighten the assembly.

The tightening of the assembly imparts a tensile stress (lbs/in2, or N/m2) in the bolt, and a compressive stress in the components being clamped between the bolt-nut assembly, or between the bolt and the component containing the threaded hole.

 

Therefore, bolt tensioning is the result of bolt torqueing.

 

Regards,

D. Thompson

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PK M
Sent: Sunday, February 25, 2018 4:06 AM
To: materials-welding@googlegroups.com
Subject: [MW:27382] Differance between Bolt Torquing and Bolt tentioning ?

 

Dears,

 

Differance between Bolt Torquing and Bolt tentioning ?

 

thanks.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...