Sunday, February 25, 2018

RE: [MW:27383] Difference between Bolt Torqueing and Bolt Tensioning

PK M,

 

Bolt torqueing refers to the circumferential moment (ft-lbs, or m-N) exerted on a bolt-nut assembly, or on a bolt and threaded-hole assembly, to tighten the assembly.

The tightening of the assembly imparts a tensile stress (lbs/in2, or N/m2) in the bolt, and a compressive stress in the components being clamped between the bolt-nut assembly, or between the bolt and the component containing the threaded hole.

 

Therefore, bolt tensioning is the result of bolt torqueing.

 

Regards,

D. Thompson

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PK M
Sent: Sunday, February 25, 2018 4:06 AM
To: materials-welding@googlegroups.com
Subject: [MW:27382] Differance between Bolt Torquing and Bolt tentioning ?

 

Dears,

 

Differance between Bolt Torquing and Bolt tentioning ?

 

thanks.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...