example 

In case PQR qualified with  preheat  of 90°C ,  your WPS  minimum preheat temperature is 35°C . your are allowed to weld decreasing 55°C.

You shall not weld preheat below or equal to 34°C.



On Mon, Feb 26, 2018 at 11:04 AM, sankar rao <sankarkorukonda@gmail.com> wrote:
Dear friends,
   Essential variable for preheat what is the meaning of
Decrease>55°c (QW406.1)


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
selastine sudhakar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...