Monday, February 5, 2018

Re: [MW:27315] regarding precautions to be taken while conducting PQR

Dear Mr. Kiran,
Below screen shoots for your reference.


Regards,
Muhammad Babur Khan


On 5 Feb 2018, at 6:32 AM, Nadakuditi kiran kumar <kinnu78@gmail.com> wrote:

dear sir's,

Material of construction is A 333 Gr 6 OR A 671 Gr CC 60



Thanks & Regards

N.Kiran kumar,
+91- 7016029043
+91- 7477799537

On 5 February 2018 at 00:33, Babur Khan <mbabur.bwp@gmail.com> wrote:
Dear Mr. Kiran,
Please share material specification.

Regards,

Muhammad Babur Khan Lashari
Sr. QA/QC Inspector (Welding)

(CSWIP 3.1 / CWI II From PWI) 

Mob: + 966 58 2774568 / 050 5193275

PAK : + 92 334 6186285 (Whatsapp)

Skype: babur.lashari


On Sun, Feb 4, 2018 at 8:17 AM, Nadakuditi kiran kumar <kinnu78@gmail.com> wrote:
Dear sirs,

We are going to conduct PQR for 3" x 5.49 mm with root ER 80S Ni1(Process - GTAW), fillup & final with E 7018 C3L (Process - SMAW) for LTCS pipe in our ongoing project. In the same project other company conduct same PQR but failed in impact test. As impact test conducted at -50 deg., Celsius.

What are the precautions to be taken to conduct PQR without fail in impact test. As we purchased our electrodes which already impact test qualified at -50  deg., Celsius. 

Appreciate your valuable suggestions.

thanks in advance  

N.Kiran kumar,
+91- 7016029043

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...