Re: [MW:27372] If a welder is qualified with SS (Stainless Steel) GTAW, He can weld CS Carbon steel GTAW?

If welder qualified with SS 
(GTAW Process),
He can weld CS ( GTAW Process)
Because of F.No's same for both SS &CS  for GTAW 
SS ---- F.NO 6.  SFA NO. 5.9
CS----- F.NO 6.   SFA NO. 5.18

On 24 Feb 2018 14:50, "'Prashant Panchal' via Materials & Welding" <materials-welding@googlegroups.com> wrote:
Since he may have used backing gas for SS gtaw he will not be qualified for carbon steel as we do not use backing gas for cs material. 
Alternatively u will have to use backing gas for cs as well


On Sat, Feb 24, 2018 at 3:33 PM, PK M
Dear Sir,

If a welder is qualified with SS (Stainless Steel) GTAW,  He can weld CS Carbon steel GTAW? Need code Referance...

Thanks.
PKM

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...