[MW:27338] Fw- Radiography of tube to tubesheet joint using rod anode method,

Dear experts,


Please advise your view on this type of radiography, has anyone in the group experienced such type of radiography, 

 

Tube sheet material- SA182 F11 with SS308L overlay,

Tube material- SA213 TP304.

Tube sheet thk- 240mm.

No of tubes are 1951, pitch is 23.81mm

Tube size- 19.05 OD x 1.65mm thk.


    

 







Regards,

Anthony.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...