Dear all,
Please advise me in below condition during review of PWHT chart construction code is ASME B31.3 with SAES-W-011.
Welding joint Material is A234 WP11 CL1 to A182 F11 CL2. Sch. S160.
Soaking temperatures is 715 'C
Soaking time 2 hrs.
Control cooling stop on 490 'C due to electrical supplies problems .
Contractor suggestions for hardness test.
Thanks and Waiting for experts views.
Regards,
M. Babur Khan
QA/QC inspector (Piping & Welding)
JAPID Jizan Refinery KSA
Cell number 00966582774568
Whatsaap 00923346186285
Sent from my iPhone
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment