Hi!
Yes Ir is always recommended to have proper uniform preheating to reduce distortion of t sht .hlgher hardness .and cracks
Regards
Hegde p b
 B


On Mon, 19 Feb 2018 at 12:04, Manoj Prabakaran.M
<manojmuthuraj955@gmail.com> wrote:
Dear sir,
I have one more doubt, we are fabricating CS heat exachanger ref construction code as asme sec viii div i.
Tubesheet thk as 150mm
Tube O.D as 30 X 2.5mm thk.
Wether preheating is required for this joint or Not before t/ts welding?
Kindly give me the solution,

MPK

--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...