Re: [MW:27327] what is the difference between d4 and d7 film

D4 Films are Extra Fine grain Film with Very High Contrast associated with High Cost and more exposure Time.


D7 Films are Fine grain Film with High Contrast and High Speed.

Thanks & Regards

J.Gerald Jayakumar

0091-9344954677



On Friday, February 9, 2018, 2:33:47 PM GMT+4, <baskarmech15@gmail.com> wrote:


Dear Expects 

how to classify the d4 and d7 film , tell the difference between two films.

Thanks and Regards
Baskar P
+91 9944876002

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...