Dear Mr.Kiran,
Greetings.Whether you carried out test at parent metal,HAZ and weld metal.If so,Can you also share the values received in parent metal,HAZ and weld metal along with Material specifications

On 04-Feb-2018 11:01 AM, "Nadakuditi kiran kumar" <kinnu78@gmail.com> wrote:
Dear sirs,

We are going to conduct PQR for 3" x 5.49 mm with root ER 80S Ni1(Process - GTAW), fillup & final with E 7018 C3L (Process - SMAW) for LTCS pipe in our ongoing project. In the same project other company conduct same PQR but failed in impact test. As impact test conducted at -50 deg., Celsius.

What are the precautions to be taken to conduct PQR without fail in impact test. As we purchased our electrodes which already impact test qualified at -50  deg., Celsius. 

Appreciate your valuable suggestions.

thanks in advance  

N.Kiran kumar,
+91- 7016029043

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...