Skip to main content

Re: [MW:23326] Painting before pressure test on pipings - B 31.3

Dear All,

Is also the the insulation (rockwool+alluminium) allowed to be on the welds during the hydrotest? 

Thanks in advance.
Best Regards,
Roger


Il giorno martedì 20 marzo 2012 13:09:13 UTC+5, madhan ha scritto:
Hi all,

Thanks for your valuable comment and now i am more clear with the particular section.

Regards,
Madhan



On Tue, Mar 20, 2012 at 1:33 PM, DOKKU AJAY <akdd83@yahoo.com> wrote:
Hi,
 
The statement "except that joints previously tested in accordance with this Code may be insulated or covered" means that if the piping is already leak tested before i.e. at a fabircation shop or at site prior to assembly, then the joints can be insulated or covered. Please note that here the code is not talking about the priming and painting. It's only about the insulatioin or covering.
 
The second statement " All joints may be primed and painted prior to leak testing unless a sensitive leak test (para. 345.8) is required." means that the joints may be primed and painted which are subjected to initial (first time) leak testing subjected to the applicability of sensitive leak test.
 
 
Dokku Ajay Kumar
Mobile: +966 500071054
 
From: Samuvel <samuvel.masilamani@gmail.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Cc: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Monday, March 19, 2012 4:57 PM
Subject: Re: [MW:13936] Painting before pressure test on pipings - B 31.3

If u have 100% joint  NDT,you can obtain a concession request from your client



On 18-Mar-2012, at 6:42 AM, madhan chozhan <madhanchozhan@gmail.com> wrote:

Gents,

Good day.

I need to know whether leak test (hydro or pneumatic) can be done on piping after painting is done on the welds of pipe line?

ASME B 31.3 says "345.3 Preparation for Leak Test
345.3.1 Joints Exposed. All joints, welds (including
structural attachmentwelds to pressure-containing components),
and bonds shall be left uninsulated and
exposed for examination during leak testing, except that
joints previously tested in accordance with this Code
may be insulated or covered. All joints may be primed
and painted prior to leak testing unless a sensitive leak
test (para. 345.8) is required."

"345.8 Sensitive Leak Test
The test shall be in accordance with the Gas and Bubble
Test method specified in the BPV Code, Section V,
Article 10, or by another method demonstrated to have
equal sensitivity. Sensitivity of the test shall be not less
than 10−3 atm·ml/sec under test conditions.
(a) The test pressure shall be at least the lesser of
105 kPa (15 psi) gage or 25% of the design pressure.
(b) The pressure shall be gradually increased until a
gage pressure the lesser of one-half the test pressure or
170 kPa (25 psi) is attained, at which time a preliminary
check shall be made. Then the pressure shall be gradually
increased in steps until the test pressure is reached,
the pressure being held long enough at each step to
equalize piping strains"

here text in green says it shall be left uncovered expect that joints previously tested in accordance with this code(which test to be done for exception and where it is mentioned on code?) but the text in red says it may be primed and painted which looks controversial, kindly advice me what to follow.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & Regards
Srirammadhan
Piping/painting inspector
Great drill Chaaya
Great Ship
Hamriyah Free zone, UAE
+971-509846269

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/951620dd-267c-4f0a-9fc5-907bcb791f4e%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...