[MW:23360] Re: Carbon pick-up in stainless steels

this is a diffusive problem, diffusion depends mainly on time and temperature CO2 from combustion is relatively stable at the temperatures in your furnace so it is more difficult to diffuse carbon in the steel.

You can measure indeed through chemical analysis if some carbon was pick up during reheating.

Sergio Muñoz
IWE-IIW
http://weld-ing.blogspot.com

On Tuesday, August 11, 2015 at 10:35:08 PM UTC-5, BM wrote:
A manufacturer of stainless steel pipes uses coal gas in reheating furnace to heat SS billets before the piercing operation. The coal gas is generated by combustion of coal in a hearth before the reheating furnace and 'simply filtered' before entry for combustion in the reheating furnace.

Is there any possibility of carbon pick-up in the billet due to the gas and other carried over products of combustion like tars etc, especially if the billet is of low carbon type?

Thanks in advance for your responses.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8c30058a-021c-45a6-a4d1-0d5a490b2dc5%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...