Inaddition to what George has highlighted
1. For a dissimilar thickness weld between Base Material 6mm thick to 19 mm thick example like a shell to dished End and a skirt to a shell.
Thanks & Regards
J.Gerald Jayakumar
0091-9344954677
From: "george.dilintas@gr.bureauveritas.com" <george.dilintas@gr.bureauveritas.com>
To: "Ri@z" <materials-welding@googlegroups.com>
Sent: Thursday, August 6, 2015 6:15 PM
Subject: Re: [MW:23280] Multiple WPS from single PQR
Many advantages like:
1. Partial penetration welds
2. Combination with other processes
3. Welding of small bore piping with GTAW
Sent from my BlackBerry 10 smartphone.
| From: Ri@z Sent: Πέμπτη, 6 Αυγούστου 2015 - 13:24 To: Materials & Welding Reply To: materials-welding@googlegroups.com Subject: Re: [MW:23276] Multiple WPS from single PQR |
Thank You For reply
My humble doubt is, 1 ) weld metal deposition is restricted to be max 6 mm for gtaw, and 13 mm for SMAW, what is the advantage of having 19 mm as Qualified base metal thickness. For separate process there is no advantage of Base metal Qualified as per QW-451 ie 1.5 to 2T
AM I RIGHT ???
On Thursday, 6 August 2015 14:02:14 UTC+5:30, George Dilintas wrote:
Backing is a welders qualification essential variable. For PQR it is a nonessential one.The Base metal qualification range is the same for the 3 casesSent from my BlackBerry 10 smartphone.
From: 'Bijay' via Materials & WeldingSent: Πέμπτη, 6 Αυγούστου 2015 - 09:55To: materials-welding@googlegroups comReply To: material...@ googlegroups.comSubject: Re: [MW:23273] Multiple WPS from single PQRThis message contains confidential information. To know more, please click on the following link: http://disclaimer. bureauveritas.com--
But for SMAW single process you have to give Metal baking as the GTAW weld Metal act as metal baking.
From:"Ri@z" <riaz.r...@gmail.com>
Date:Thu, 6 Aug, 2015 at 11:58 am
Subject:[MW:23271] Multiple WPS from single PQR--Dear Sir,,I have one PQR with 3 mm GTAW weld deposit and 6.5 mm SMAW deposit. Base metal thickness is 9.5 mm and impact is not required.Please correct me if any of the following is NOT correct as per Sec IX1) Combined Process (GTAW + SMAW) up to a thickness of 1.5 to 19 MM (2T)2( Single process wps of SMAW with weld metal thicjness 13 MM and qualified base metal thickness is 1.5 mm to 13 mm3) Single process WPS of GTAW with weld metal thickness of 6 MM and Qualified base metal thickness is 1.5 to 6 mmPlease help!!Riaz
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
To post to this group, send email to materials-welding@ googlegroups.com.
Visit this group at http://groups.google.com/ group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/ msgid/materials-welding/ b3a24345-befb-4d5c-b65a- 9cfc47a53889%40googlegroups. com.
For more options, visit https://groups.google.com/d/ optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@ googlegroups.com.
To post to this group, send email to material...@ googlegroups.com.
Visit this group at http://groups.google.com/ group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/ msgid/materials-welding/ 1438843327.97025. YahooMailAndroidMobile% 40web181301.mail.ne1.yahoo.com .
For more options, visit https://groups.google.com/d/ optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cba069da-c9e1-4902-9e1d-bbefd56859c0%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20150806124506.6459476.32204.12249%40gr.bureauveritas.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20150806124506.6459476.32204.12249%40gr.bureauveritas.com.
For more options, visit https://groups.google.com/d/optout.
Comments