Re: [MW:23338] Tungsten inc. API 1104

​​Tungsten inclusion is not defined as a defect as per API 1104, however it is often considered a volumetric imperfection and is accepted or rejected accordingly.

regards,
LALU


LALU


On Mon, Aug 24, 2015 at 7:06 AM, Mehdi Vafakhah <mehdi.vafakhah@gmail.com> wrote:
Dear experts

What's the Acceptance of tungsten inc.
According to  1104?
Method: RT

Regards

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f43bf2b3-c38d-4fd1-b4ad-b2ae6d24a18a%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOwU13tYHcn9J%2B-kd9Bj%3D6Ne7SHWVjxJ94%2BygPWJkNVG-99VHQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...