Wednesday, August 19, 2015

Re: [MW:23310] S.A. 2.5 surface profile

Dear Jasim,

SA 2.5 is a degree of cleanniness as per  ISO 8501-1.This much of cleanniness is sometimes required for joint wrapping.Yes you can achieve SA2.5 through sand blasting but this is banned all across world.
Surface anchor profile is different thing which is measured in either microns or in mills and Not required for joint wrapping.


Regards,
Kalimullah

On Tuesday, August 18, 2015, Jasim Ahmed <jasim.kuet.me@gmail.com> wrote:
Dear experts,

I badly need to know - is it possible to create S.A. 2.5 surface profile for joint wrapping without sand blasting?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5e6cfb73-db6b-48b1-8dbe-a7bb3f93f062%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOXPmDtNoWos96P%2BjBNY7GBgu%3DaRnwBW%3DGsQ%2B9_MMWA-zHWnDA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...