Re: [MW:23314] Brass versus Bronze as an Alloy for High chlorine service

Hi Arunabh,

As per the fire norms NFPA-13, 4 way and hydrant valves are brass MOC. Brass valves are acceptable. 

Regards,

Mahek shah
Assist. Manager QA/QC
Larsen & Toubro Ltd

On Tue, Aug 18, 2015 at 3:31 PM, ARUNABH BERA <bonjoe23@gmail.com> wrote:

Dear Sirs
In our Project, fire water valves and hydrants are generally specified as SS-316 because of their high ability to resist pitting resistance in Chlorine environment. However the client is insisting to use either Brass or Bronze as MOC for all Valves internals. Kindly guide me which is more superior Brass or Bronze in terms of its resistance to SCC, weldability and other issues
Supporting references for the above would be helpful

Regards
Arunabh
Project Co-ordinator
Engineers India Limited

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/95a4570e-daed-4d7b-9dd7-078ab6a7c37d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BtkXLTKKD5EXWdgwHty7QtYQe_XmO31Qa893M0gO4AztgcijQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...