Re: [MW:23357] Welding consumables (2.25Cr-1Mo-0.25V) with guaranteed stress rupture strength

Hi,
Your  query  is too general. What's the design code ,design  specifications  and intended applications ? To the best of my knowledge,  these steels  are used  for hydroprocessing equipments. 
Appreciate your response with more details.

Thanks. 

P.Goswami. 


-------- Original message --------
From: "S.Mohammed" <mohd52100@gmail.com>
Date: 2015-08-26 20:54 (GMT-07:00)
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:23352] Welding consumables (2.25Cr-1Mo-0.25V) with guaranteed stress rupture strength

Expert opinion needed.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/27b7de07-9427-4e41-92b0-125ff396af62%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...