[MW:23308] RE: 23305] S.A. 2.5 surface profile

SA 2.5 is, by definition a grit blast finish – so the answer is no.

 

Alan Denney

AKD Materials Consulting Ltd

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Jasim Ahmed
Sent: 18 August 2015 08:00
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:23305] S.A. 2.5 surface profile

 

Dear experts,

 

I badly need to know - is it possible to create S.A. 2.5 surface profile for joint wrapping without sand blasting?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5e6cfb73-db6b-48b1-8dbe-a7bb3f93f062%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...