Thursday, August 13, 2015

[MW:23300] Re: cracke- Moc ss cap thk-2.5 mm

what is the service and operating parameters(pressure and temp) . And are u sure that it had occurred in service and is not a manufacturing defect ? 

On Saturday, 8 August 2015 10:08:27 UTC+5:30, Kunal Patel wrote:
dear expert,

pl. review the attached photo first. let me know, what are the causes for crack developed in weld joints between cap to condenser flange ?
I observed crack at fillet weld joints (partition plate to cap inside surface) - how it was occurred ? would both cracks be intersected from inside ?

your valuable reply will be appreciable.

r/s
Kunal Patel
Bureauveritas

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/874887c0-04b5-435b-8ea9-c7a5e19eaad1%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...