HI, the word SA denotes for blast cleaning,
Further details of 2.5grade, achieving profile, for which application will all come at later on...

Lakshman kumar.B
Project manager.
9440031459

From: Jasim Ahmed
Sent: ‎18-‎08-‎2015 12:34
To: Materials & Welding
Subject: [MW:23305] S.A. 2.5 surface profile

Dear experts,

I badly need to know - is it possible to create S.A. 2.5 surface profile for joint wrapping without sand blasting?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5e6cfb73-db6b-48b1-8dbe-a7bb3f93f062%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...