Re: [MW:23349] Grade of MATERIAL

Dear Ali

1 - Please check chemical analysis of tested samples. Specially carbon content and also carbon equivalent provides more data for grade identification. It should be with regards to that, if those pipe are welded or seamless. 

2 - Review sampling position, number of samples and their standard type (rectangular or round) according to the standard.

3 - For PSL2 there is more tests defined in the standard for better grade identification, however those tests are for certifying PSL2 and have not been defined for grade details, but they may help you to find the best matched grade.

4 - Eventually, it is probable that the pipe covers 1, 2 or more grades. The permission for use should be based on engineering data. For example, lower carbon equivalent is better for welding and higher cavbon equivalent may cause using pre-heat and PWHT.


Regards

On Wed, Aug 26, 2015 at 1:04 PM, Ali Asghari <asgharialigl@gmail.com> wrote:

Dear All.
In material specification such as API 5L, minimum yield strength specified (in some cases maximum yield strength also given) that cause a wide range that overlaps with other grades.

Now with regard to attached  mechanical testing  result of some materials, contractor insist that these materials are X52(due to their wps can support them) but strength of them is near to X60 and X65.
How it could be clarified?

Regards.

---------- Forwarded message ----------
From: "Ali Asghari" <asgharialigl@gmail.com>
Date: Aug 21, 2015 7:34 AM
Subject: UNKNOWN MATERIAL
To: <materials-welding@googlegroups.com>
Cc:

Dear All.
In material specification such as API 5L, minimum yield strength specified (in some cases maximum yield strength also given) that cause a wide range that overlaps with other grades.

Now with regard to attached  mechanical testing  result of some materials, contractor insist that these materials are X52(due to their wps can support them) but strength of them is near to X60 and X65.
How it could be clarified?

Regards. 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALcH7WBUQ8pa7Uh5AOtUadpqsy21jBNXMW99trHybuY8rQr1EQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer

Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023




--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC8uMtsQQ-ZKco8OPF5-WSrY4%3DkTt1SQ4nYAifxPM_j2DMe5kw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...