[MW:23293] WPS Supplementary essential variable for Impact

Dear sir,

I have PQR for P1 G1 to P1 G2 as per Impact test requirement  G no. is supplementary essential variable.
My question is can I made P1 G1 to P1 G1 & P1 G2 to P1 G2 wps using same PQR without change in other essential & supplementary variable.

No comments:

Re: [MW:35686] HDPE WPS