 Dear  Members,
 
I had a doubt about TTS joint mockup pullout test , as per the configuration no welding only expnansion , let me know the fr. value for that.
 
Best regards 
 
Thiyanes G  
On Monday, January 12, 2015 at 11:25:11 AM UTC+5:30, silambarasan veluchamy wrote:
Dear members,
We are going to carry out a Mockup Procedure qualification for T-TS joint as per ASME SecIX. what are the test required to carry for the qualification. I hear from a TPI that RT, Tear test & pull out has to be carried out, whereas ASME Sec IX & Tema class 'R' are not talking about the above said tests. 
Is the above said tests required? If so, the as per which standard?
Kindly advice

BR,
M.V.Silambarasan

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bdc8af70-c418-4149-8a5f-8a51b0ae6569%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35763] Hardness range for CS+ Alloy0625 clad welding

Dear experts. I am currently in the process of qualifying a PQR for API 5L X65 + A350 LF6. Both material consists of a base metal with alloy...