Re: [MW:23125] Re: ASME UG-10 interpretation

you will not have to recertify the material.  For example, please read Section VIII Division I Nonmandatory Appendix 43 and specifically 43-3-3 (similar instruction for Sc I).  This directs you to ASME Section II-Part A but not very cleanly.  You will need to go to Mandatory Appendix II.  This appendix has a table of all ASME/ASTM specifications and the acceptable Code editions for each and any additional notes.  For SA/A-516 the entry is on page 1762 of Section II Part A, 2nd volume.


Hope this helps.



From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> on behalf of Prakash Gotimukul <gprakash31@gmail.com>
Sent: Tuesday, June 30, 2015 12:57 AM
To: materials-welding
Subject: Re: [MW:23124] Re: ASME UG-10 interpretation
 
Code edition applied includes material also. 2013 edition gives details of how to accept material of earlier/later editions of code. Pl refer appendices

Rgds
G.Prakash
AIS, AIA LLC TX, USA
Tel: +9714 2778511 Mob:+97152 979 5678

On Mon, Jun 29, 2015 at 11:55 AM, Vishnu GK <vgkp88@gmail.com> wrote:
plate astm 516 to sOn Thursday, May 7, 2015 at 9:07:26 PM UTC+4, New91 wrote:
> Reviewing a material test report (MTR) of SA-516-70 certified as per ASME 2010 Ed 2011àddenda and MTR complies with all the requirements. The Job is to be U stamped per ASME 2013 ED. Theres no requirement of materials to be certified to làtest code editions in contractual documents. Since job is to be code stamped per 2013 Ed, should material also be recertified as per ASME 2013 Ed?

I Need to recertify Astm 516 to sa 516.can Anyone provide me a recertification format for this.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7120b3b3-2b8e-411b-8903-438b5613e5d5%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOUP4q%2B4h335ZZ1vHU8Bn8_ETLThJQp-cTryTB%3DQ53%2BDKsEr6w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...