Re: [MW:23121] Article 344.5.2 specifies 100% radiography for girth and miter groove welds in paragraph - Reference to definition of "Girth and Miter Groove welds"

Miter and girth means angle in circumferencial in weld to bend the the pipe it should be less than 15 degree.

M.Usman
Welding engineer
API 577, AWS CWI, API 510
Descon Engineering Ltd

On Jun 28, 2015 2:31 AM, "John Henning" <jhenning@deltak.com> wrote:

circumferential welds in pipe 

mitered welds still circumferential but cut on an angle to make a bend.




From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> on behalf of Oscar Artica <oscarartica@gmail.com>
Sent: Friday, June 26, 2015 9:11 AM
To: materials-welding@googlegroups.com
Subject: [MW:23119] Article 344.5.2 specifies 100% radiography for girth and miter groove welds in paragraph - Reference to definition of "Girth and Miter Groove welds"
 
Hello Experts,

Could anyone explain what the definition of "Girth and Miter" groove welds are? I can't seem to find the definition anywhere and only mentioned in this passage of B31.3. Thanks!


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/45f8412f-e4a0-4d9b-ac6d-ae3991a2bdf0%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/BL2PR03MB274AE677A1EA21A8F4B7FD5A1AC0%40BL2PR03MB274.namprd03.prod.outlook.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BhbQbvH53Aah4npcJLcOpDiw0Z4hvwC1zaOV9cuDqwBYDhtCQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...