Dear Mr. Jayakumar,
Thanks for your valuable reply. For fossil power plant,there is any applicable code for particular issue.
Regards
On Tue, Jun 23, 2015 at 11:38 AM, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
--Please refer API Recommended Practice 934-A regarding Post Heating or DeHydrogenation TreatmentRecommended 300degC for min 1Hour.Copy not available with me.Thanks & RegardsJ.Gerald Jayakumar0091-9344954677
From: pradip kumar Sil <pradipsil@gmail.com>
To: materials-welding <materials-welding@googlegroups.com>
Sent: Tuesday, June 23, 2015 9:57 AM
Subject: [MW:23103] Post Weld Hydrogen bake out...Post weld baking -P-22
--Dear All,Post weld hydrogen bake out ( Post weld baking ) is aplicable for ASTM 335 GR. P-22 material.There is any applicable standard.RegardsPradip
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8%3DCaX1AdqLcBxo0Ni8xeX8EnyQZ7tq8zv6eOE9Ovf7hXQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/561924799.3748955.1435041510885.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8kk%3DXOkU-JBcTMC-T-AdnFnazyPiSwu5wDuHyMgjPU8JA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments