Monday, June 22, 2015

Re: [MW:23101] Doglegs Tolerance

Can you specify the pipe spec and what it is used for ? Since you are referring to "line pipe" I presume its the pipe covered in spec API 5L. 
 


On Wed, Jun 17, 2015 at 4:04 PM, krishna kamal nayan Pandey <kkmech1987@gmail.com> wrote:
Can any body gives permissible tolerance for Dog leg. Whether any standard is covering this tolerance.
 

Best Regards,

 

Krishana Kamal Nayan

QA/QC  Engineer

Weatherford Oil Tool Middle East Ltd. |

Mobile:+964 780 925 0270

Krishana.Nayan@ME.Weatherford.com  │ www.weatherford.com

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN%2Bgo9CfWqhkWxW80UBPPdRTi4ex%3D5VWFh_yCtkopBzMrA_q2A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2Bmi6Ge2mbmxcLm0ZogxejyGG2xh1LqpWET809PxGcFTqLwqgg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.