Friday, June 19, 2015

Re: [MW:23094] Reduce silicon content

Guys I face high silicon content in ER70S-3 with high rejection repair rate,after changing of ER70S-6 we reduce repair rate.better purchase different manufacturer,and verify purging gas purity.

On Wednesday, June 17, 2015, Anup N K E <nkeanup@gmail.com> wrote:

Replace ER 70S-6 with ER70S- 3 GMAW filler wire. Silicon content is 0.45 % to 0.75% for ER70S-3  and 0.8 % to 1.15 % for ER 70S- 6.

This is as per Aramco recommendation.

Regards,

Anup

On 17 Jun 2015 06:57, "Pravin G" <htcispravin@gmail.com> wrote:
Dear Expert

Welding application: compressor piping
Process: GMAW 1.2mm ER70S-6
Welding issue: silicone contamination after welding

How can I reduce the silicon content?
Any special method or consumable which can solve this issue?

Kindly advice.

Pravin Poornachandran
Singapore

Sent from my iPhone

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7941CE40-4030-4247-AABE-EB015A292649%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJsQutbzSCJZTnrU3Q3Rzh0%3DjKtubQx_bkHLEh2SUgHJWBdz1A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


--
With Best & Regards

N.Srinivas,
Welding Inspector,
0561198050,0537812787
Al-Khobar.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABMP0bNc%2BzMu3RP4Gnf72Xuqk91%2BmtxyrYbOQNdFxKAc88Y8Pg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...