Re: [MW:23079] Reduce silicon content

change over to another consumable manufacture

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Wed, Jun 17, 2015 at 1:58 PM, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
is it like a slag?? at random

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Wed, Jun 17, 2015 at 12:07 PM, Ahmad el-sharkawy <ahmad.sharkawy88@gmail.com> wrote:
can you send chemical composition of piping and welding electrode also? and tell us what is problems and percent of silicon at weld metal?

On Tue, Jun 16, 2015 at 5:49 AM, Pravin G <htcispravin@gmail.com> wrote:
Dear Expert

Welding application: compressor piping
Process: GMAW 1.2mm ER70S-6
Welding issue: silicone contamination after welding

How can I reduce the silicon content?
Any special method or consumable which can solve this issue?

Kindly advice.

Pravin Poornachandran
Singapore

Sent from my iPhone

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7941CE40-4030-4247-AABE-EB015A292649%40gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
WITH MY BEST WISHES

AHMED ELSHARKAWY
QA/QC ENGINEER
DIPLOMA DEGREE IN WELDING ENGINEERING.
CERTIFIED WELDING INSPECTOR " CWI " 14072901.
ASNT LEVEL II " RT&VT&UT&PT&MT"
IRECA CERTIFIED LEAD EDITOR ISO 9001/2008.
PREPARING MASTER DEGREE IN WELDING ENGINEERING.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK-7o_NV%2BxMwSKcTOBoqi86g%2B86_kpZ_3ifOYDM6-di1U43H7g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePPFSzQy4cYUb-w-rfEQCJ%2B5gByGUUjHzg-4b8MDGN3Fw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.