Re: [MW:23078] Reduce silicon content

can you send chemical composition of piping and welding electrode also? and tell us what is problems and percent of silicon at weld metal?

On Tue, Jun 16, 2015 at 5:49 AM, Pravin G <htcispravin@gmail.com> wrote:
Dear Expert

Welding application: compressor piping
Process: GMAW 1.2mm ER70S-6
Welding issue: silicone contamination after welding

How can I reduce the silicon content?
Any special method or consumable which can solve this issue?

Kindly advice.

Pravin Poornachandran
Singapore

Sent from my iPhone

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7941CE40-4030-4247-AABE-EB015A292649%40gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
WITH MY BEST WISHES

AHMED ELSHARKAWY
QA/QC ENGINEER
DIPLOMA DEGREE IN WELDING ENGINEERING.
CERTIFIED WELDING INSPECTOR " CWI " 14072901.
ASNT LEVEL II " RT&VT&UT&PT&MT"
IRECA CERTIFIED LEAD EDITOR ISO 9001/2008.
PREPARING MASTER DEGREE IN WELDING ENGINEERING.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK-7o_NV%2BxMwSKcTOBoqi86g%2B86_kpZ_3ifOYDM6-di1U43H7g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...