Re: [MW:23075] Multiple specimen - Tensile test location - ASME SEC IX - QW 151- Sub clause - c , d,

Dear Sir,

According to QW-151.2(d),
when multiple specimens are necessary, the entire thickness shall be mechanically cut into a minimum number of approximately equal strip of a size that can be tested in the available equipment.
So in your case Pipe thickness is 40 mm so size of multiple specimen shall be 20 mm (Top) and 20 mm (bottom)

Regards,
Navnitkumar Parikh

On 15 Jun 2015 22:40, "Vishwas Keskar Welding Manager Pune India" <vvkeskar123@gmail.com> wrote:
Dear Experts ,

 40 mm thk pipe test coupon of  PQR was welded using GTAW + SMAW process .For tensile test specimens,test pieces are required to draw as Multiple specimens to represent full thickness .The specimen locations were marked on the pipe as per ASME Figure.
While  drawing the specimens , the specimens were machined from the  marked locations on pipe . However it is observed that the specimen(Top and Bottom ) are not got machined exactly one below each other but a little offset.The bottom specimen is a little offset  to Top side specimen.

 The Top side specimen thickness was 25 mm and bottom side specimen was also 25 mm .But inactual the thickness of the test pipe is 40 mm .
.In total , full thickness representation shall not be more than 40 mm . Actually it 25 + 25 = 50mm. So the query.

But at the outset ,Collectively , the full thickness tensile testing is achieved as per Code
(Two location  - One set - Top tensile 1 , Bottom Tensile 1 -
Other set - One set - Top tensile 2 , Bottom Tensile 2

Side bends are satisfactory as per Code

Question :

 Is the intent of the Code that the specimen shall be drawn exactly one below each specimen(Bottom side specimen exactly below the top side specimen) to represent the full thickness or some offset is acceptable to represent the full thickness as mentioned above
.

Regards


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/58df1d33-9862-4efd-a4d9-12c5192e44ee%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKHZGHqoMwCBfU0qqZ%2BcQghe5pBOywF0ePNAYqcj_xrmqQ7U4g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...