Re: [MW:23071] centreline crack

what s ur joint design? if it is double bevel whether 1/2 on both sides or 2/3 & 1/3 ? preheat temperature?

On Sat, Jun 13, 2015 at 11:02 AM, Gigin Gumilar <giginsg@gmail.com> wrote:
Dear expert,

Any suggestion to prevent centreline crack? i was found centreline crack exist on the first run/layer after backgouging.
base material is S355JR 50mm thick with joint configuration double bevel tee joint full-pen weld by SAW.

Thank you for your help

Rgds,
Gigin

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5472638b-731d-405b-b158-0ef2e503b08b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
G.Gopalakrishnan
Welding Engineer
Mukand Ltd
Mumbai
Moble :+91-9833397917

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOp_kKhV2xOVqfzAKmd8ofwYC1PG%3D9FMRR49Y4fsWjUa%3D6%2BUzw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...