Re: [MW:23068] RT Report clarification / advise required

Dear Friends,
 
As per my understanding ASNT level - II have one qualification for  Radio Graphic Inspection which is ASNT LEVEL -II - RT.
which covers film review and reporting.
 
For Radio graphic film interpretation & Report authorization requires  ASNT LEVEL -II - RT.
 
The other qualification like MPI or LPE a level 1 operator can do that performing the MPI or LPE. Report evaluation and authorization by ASNT LEVEL -II MPI or LPE
 
But in RT film review Level-I cannot do.( Mostly in Middle east we are using Level- II for all including preforming MPI / LPE )
 
 
Kingsly Geo
Bureau Veritas
Abu Dhabi

On 13 April 2015 at 12:27, Hareesh K V <hareesh13h@gmail.com> wrote:

Dear sir,

Please share with the vendor the guidelines of ASNT about level 2 in RT and RTFI.

RT qualification from ASNT Level 2 is an operator level qualification. In INDIA, an ASNT level 2 person cannot operate a radiography camera as we have to follow the regulations of AERB .Outside INDIA an ASNT level 2 person can operate a radiography camera.

In ASNT level 2 in RT there is nothing regarding the evaluation of radiography film.

An ASNT RTFI level 2 person is qualified to evaluate Radiography film, interpret it and is qualified to sign the report.

It is a general perception that an ASNT Level 2 in RT is qualified for film interpretation and that is wrong.

Best regards,

Hareesh K V

On Apr 13, 2015 11:07 AM, "Mohammed Ismail" <mohammedismail.inspections@gmail.com> wrote:
Dear Sir,

This are RT report - final evaluation report / RT review form in which result of the RT were mentioned. Not the films.

For information these reports which is subjected for review were for the castings (eg; valve body /pump casing / cover).

with regards,
Mohammed Ismail

Thanks & Best Regards,

Mohammed Ismail

Inspection Engineer-Mechanical

Phone : +966 38394292 Ext - 243

Mobile + 966 565 063 994

Fax : + 966 3 8393671 

Velosi Saudi Arabia

Dammam-KSA.


On Thu, Apr 9, 2015 at 3:17 PM, safad pp <safadpp@gmail.com> wrote:
Dear Ismail,

please let us know whether  you reviewed  RT Report or RT film ? In
your quote  RT report is mentioned only...

Shafad P.P
ASNT LEVEL 111 (RT,UT& MT)
India

On Wed, Apr 8, 2015 at 11:45 PM, Mohammed Ismail
<mohammedismail.inspections@gmail.com> wrote:
> Dear Experts,
>
>
>
> I am pleased to draw your attention and please provide your valuable input /
> advice / comment / clarification regarding my interpretation as below.
>
>
>
> The following is the requirement as referring to the attached 6600028289
> (OOK) schedule Q_quality requirements attachment 1 clause 2.2.1.
>
>
> Quote starts
>
>
> " When performing, reviewing or ensuring Nondestructive Testing in VT, MT,
> PT, RT or UT, he shall be certified in the specific method(s). When
> performing, reviewing or ensuring Radiographic Testing Film Interpretation
> (), Inspector shall be certified in ASNT Level II."
>
>
> Quote Ends
>
>
>
> My interpretation is RT report shall be reviewed or ensured by the inspector
> with ASNT Level II certified in RTFI.
>
> And after reviewing or ensuring the reports as per the requirements that
> report shall endorsed (singed) by that inspector who is qualified in RTFI .
>
>
> But the vendor is dis agreeing with the my statement.
>
>
>
> Please advise me.
>
>
> Thanks and best regards,
>
> Mohammed Ismail,
>
> Mechanical Inspector,
>
> vendor inspection department,
>
> Velosi.
>
> --
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> To post to this group, send email to materials-welding@googlegroups.com.
> Visit this group at http://groups.google.com/group/materials-welding.
> To view this discussion on the web visit
> https://groups.google.com/d/msgid/materials-welding/CAF2Z%3DtU1K6RTNjHkkjN1ibYNxK3VNSufzza5j4BgLah%2Bx%2BYAJg%40mail.gmail.com.
> For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOWuSzEttudxDmfd38WGKaKMXop%3DkpUTM-RFDMwVFJGqq255Rg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF2Z%3DtWUy2238E%3DH9Qjee4fj5gszGVbDcB01a%3D%2BpOyPC7nSZuA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM3LgAUuVqzEDmm%2BfeE%3DM%2BFY4KtM1CtmJ3Y-Hp%3DavwQy%3DKrroA%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAR7VZ_gfdStK48Wcb71Ef%2BFRqMc2fgDYjf8u2VPEC3x5srckg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...