Tuesday, June 2, 2015

Re: [MW:23059] Weldability of API 5L and P355 NL1

Comparable steel specifications

Although it is not uncommon to see this on steel company web sites, any suggestion that one steel specification and grade is an equivalent to another should be treated with caution especially because of differences in the methodology and techniques used for testing. However EN 10028:3 P355NL2 is broadly similar to the following steel specifications:

ASME SA516 Gr. 70          BS 1501 224 490B LT50

Plates certified to these standards are held in stock by Brown McFarlane.

For more information please contact our sales teams. Click here to go to the page giving contact details.


http://www.brownmac.com/products/pressure-vessel-steel-plate/en-10028-3-p355nl1-and-p355nl2.aspx



2015-06-02 8:12 GMT-05:00 'raouf salhi' via Materials & Welding <materials-welding@googlegroups.com>:
Dear expert ,

We have to weld API 5L Gr X 60 with P355 NL1, our client is asking of the weldablity of this two materials .

I'm trying to find ASME equivalent for P 355 NL1 but without results.

Regards

SALHI Raouf
QA/QC Engineer

Tel: Morocco +212628979891
      Tunisia +21621458258

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1918751175.5427834.1433250720453.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.



--

Ing. Jose Juan Jimenez Alejandro

Cel. 8110834207; Next 16789654; ID 42*15*153815

Skype: jjjimeneza

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5Zur%2BmeE8ibrrt9Enwcfb_H2FS%2BV1%3DssSKuPYGC4%3DmgLbqeg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...